A pad refurbisher that provides in situ, real-time conditioning and/or cleaning of a polishing surface on a polishing pad used in chemical-mechanical polishing of a semiconductor wafer and other microelectronic substrates. The pad refurbisher has a body adapted for attachment to a wafer carrier of a chemical-mechanical polishing machine, and a refurbishing element connected to the body. The body has a distal face positioned proximate to a perimeter portion of the wafer carrier and facing generally toward the polishing surface of the polishing pad. The body travels with the wafer carrier as the wafer carrier moves over the polishing pad. The refurbishing element is connected to the distal face of the body so that the refurbishing element can operatively engage the polishing surface substantially adjacent to the perimeter of the wafer carrier. The refurbishing element is a pad conditioning device and/or a pad cleaning device that conditions and/or cleans the polishing surface of the pad to remove waste particles from the polishing surface of the polishing pad and place the pad in a desired polishing condition. In operation, the refurbishing element travels with the wafer carrier and is selectively engaged with the polishing surface while the wafer carrier presses the wafer against the polishing surface to selectively condition and/or clean generally only the deteriorated areas on the pad.
|
0. 45. A method for refurbishing a polishing pad, comprising the steps of:
providing a pad refurbisher attached to a wafer carrier, the pad refurbisher having a first ring bearing a first refurbishment element and a second ring bearing a second refurbishment element,
selectively engaging one of the first and the second refurbishing elements with the polishing pad; and
moving at least one of the wafer carrier and the polishing pad with respect to the other to pass at least one of the refurbishing elements across the polishing pad.
0. 65. A method for refurbishing a polishing pad, comprising the steps of:
providing a pad refurbisher attached to a wafer carrier, the pad refurbisher having a body including a first ring bearing a first refurbishment element and a second ring bearing a second refurbishment element, the body being movably attached to the wafer carrier;
selectively engaging one of the first and the second refurbishing elements with the polishing pad; and
moving at least one of the wafer carrier and the polishing pad with respect to the other to pass at least one of the refurbishing elements across the polishing pad.
25. A method for refurbishing a polishing pad, comprising the steps of:
providing a pad refurbisher having a body including a first ring and a second ring each with a face positioned proximate to a perimeter portion of a wafer carrier of a chemical-mechanical polishing machine and facing generally towards the polishing surface, and a first refurbishing element connected to the face of the body first ring and a second refurbishment element connected to the face of the second ring, the body being movably attached to the wafer carrier;
selectively engaging the pad one of the first and the second refurbishing element elements with the polishing pad; and
moving at least one of the wafer carrier and the polishing pad with respect to the other to pass at least one of the refurbishing element elements across the polishing pad.
0. 41. A polishing machine for chemical-mechanical polishing of a semiconductor wafer, comprising:
a platen having an upper surface;
a polishing pad positioned on the upper surface of the platen, the polishing pad having a polishing surface facing away from the platen,
a wafer carrier for carrying the wafer; and
a pad refurbisher having a body attached to the wafer carrier, the body including a first ring having a first refurbishment element and a second ring having a second refurbishment element, the first operably coupled to a first linear actuator configured to independently move the first ring downwardly to selectively engage the first refurbishment element with the polishing surface and upwardly with respect to the wafer carrier and the second ring to selectively disengage the first refurbishment element from the polishing surface and the second ring operably coupled to a second linear actuator configured to independently move the second ring downwardly to selectively engage the second refurbishment element with the polishing surface and upwardly with respect to the wafer carrier and the first ring to selectively disengage the second refurbishment element from the polishing surface, the first ring being positioned radially outward from the perimeter of the wafer carrier and the second ring being positioned radially outward from the first ring.
0. 61. A polishing machine for chemical-mechanical polishing of a semiconductor wafer, comprising:
a platen having an upper surface;
a polishing pad positioned on the upper surface of the platen, the polishing pad having a polishing surface facing away from the platen;
a wafer carrier for carrying the wafer; and
a pad refurbisher having a body including a first ring bearing a first refurbishment element and a second ring bearing a second refurbishment element, the body being movably attached to the wafer carrier, the first ring operably coupled to a first linear actuator configured to independently move the first ring downwardly to selectively engage the first refurbishment element with the polishing surface and upwardly with respect to the wafer carrier and second ring to selectively disengage the first refurbishment element from the polishing surface and the second ring operably coupled to a second linear actuator configured to independently move the second ring downwardly to selectively engage the second refurbishment element with the polishing surface and upwardly with respect to the wafer carrier and the first ring to selectively disengage the second refurbishment element from the polishing surface, the first ring being positioned radially outward from the perimeter of the wafer carrier and the second ring being positioned radially outward from the first ring.
0. 31. A pad refurbisher for refurbishing a polishing surface on a polishing pad used in chemical-mechanical polishing of a semiconductor wafer, comprising:
a body adapted for attachment to a wafer carrier of a chemical-mechanical polishing machine with the body having a first ring and a second ring each with a face positioned proximate to a perimeter portion of the wafer carrier and facing the polishing surface of the polishing pad; and
a first refurbishment element connected to the face of the first ring and a second refurbishment element connected to the face of the second ring, the first ring operably coupled to a first linear actuator configured to independently move the first ring downwardly to selectively engage the first refurbishment element with the polishing surface and upwardly with respect to the wafer carrier and the second ring to selectively disengage the first refurbishment element from the polishing surface and the second ring operably coupled to a second linear actuator configured to independently move the second ring downwardly to selectively engage the second refurbishment element with the polishing surface and upwardly with respect to the wafer carrier and the first ring to selectively disengage the second refurbishment element from the polishing surface, the first ring being positioned radially outward from the perimeter of the wafer carrier and the second ring being positioned radially outward from the first ring, the first and the second refurbishing elements being adapted to engage the polishing surface substantially adjacent to the perimeter portion of the wafer carrier.
0. 52. A pad refurbisher for refurbishing a polishing surface on a polishing pad used in chemical-mechanical polishing of a semiconductor wafer, comprising:
a body adapted for attachment to a wafer carrier of a chemical-mechanical polishing machine with the body having a first ring and a second ring each with a face positioned proximate to a perimeter portion of the wafer carrier and facing the polishing surface of the polishing pad, the body being moveably attached to the wafer carrier; and
a first refurbishment element connected to the face of the first ring and a second refurbishment element connected to the face of the second ring, the first ring operably coupled to a first linear actuator configured to independently move the first ring downwardly to selectively engage the first refurbishment element with the polishing surface and upwardly with respect to the wafer carrier and the second ring to selectively disengage the first refurbishment element from the polishing surface and the second ring operably coupled to a second linear actuator configured to independently move the second ring downwardly to selectively engage the second refurbishment element with the polishing surface and upwardly with respect to the wafer carrier and the first ring to selectively disengage the second refurbishment element from the polishing surface, the first ring being positioned radially outward from the perimeter of the wafer carrier and the second ring being positioned radially outward from the first ring, the first and the second refurbishing elements being adapted to engage the polishing surface substantially adjacent to the perimeter portion of the wafer carrier.
1. A pad refurbisher for in situ, real-time refurbishing of a polishing surface on a polishing pad used in chemical-mechanical polishing of a semiconductor wafer, comprising:
a body adapted for attachment to a wafer carrier of a chemical-mechanical polishing machine with the body having a first ring and a second ring each with a face positioned proximate to a perimeter portion of the wafer carrier and facing the polishing surface of the polishing pad, the body being adapted to travel with the wafer carrier as the wafer carrier moves over the polishing pad wherein the body is movably attached to the wafer carrier; and
a refurbishing element connected to the face of the body a first refurbishment element connected to the face of the first ring and a second refurbishment element connected to the face of the second ring, the first ring operably coupled to a first linear actuator configured to independently move the first ring downwardly to selectively engage the first refurbishment element with the polishing surface and upwardly with respect to the wafer carrier and the second ring to selectively disengage the first refurbishment element from the polishing surface and the second ring operably coupled to a second linear actuator configured to independently move the second ring downwardly to selectively engage the second refurbishment element with the polishing surface and upwardly with respect to the wafer carrier and the first ring to selectively disengage the second refurbishment element from the polishing surface, the first ring being positioned radially outward from the perimeter of the wafer carrier and the second ring being positioned radially outward from the first ring, the first and the second refurbishing element elements being adapted to engage the polishing surface substantially adjacent to the perimeter portion of the wafer carrier and traveling with the wafer carrier while the wafer carrier moves the wafer over the polishing surface.
13. A polishing machine for chemical-mechanical polishing of a semiconductor wafer, comprising:
a platen having an upper surface;
a polishing pad positioned on the upper surface of the platen, the polishing pad having a polishing surface facing away from the platen,
a wafer carrier for carrying the wafer, the wafer carrier being positioned over the polishing pad and moveable along an axis substantially normal to the upper surface of the platen to engage the wafer with the polishing pad, wherein at least one of the platen and the wafer carrier moves with respect to the other to impart relative motion between the wafer and the polishing pad; and
a pad refurbisher having a body including a first ring and a second ring each with a face positioned proximate to a perimeter portion of the wafer carrier and facing generally towards the polishing surface and a refurbishing element connected to the face , the first ring having a first refurbishment element connected to the face thereof, the first ring operably coupled to a first linear actuator configured to independently move the first ring downwardly to selectively engage the first refurbishment element with the polishing surface and upwardly with respect to the wafer carrier and the second ring to selectively disengage the first refurbishment element from the polishing surface and the second ring having a second refurbishment element connected to the face thereof, the second ring operably coupled to a second linear actuator configured to independently move the second ring downwardly to selectively engage the second refurbishment element with the polishing surface and upwardly with respect to the wafer carrier and the first ring to selectively disengage the second refurbishment element from the polishing surface, the first ring being positioned radially outward from the perimeter of the wafer carrier and the second ring being positioned radially outward from the first ring, the body being attached to the wafer carrier so that the body and the first and the second refurbishing element elements travel with the wafer carrier as the wafer carrier moves with respect to the polishing pad, wherein the first refurbishing element engages the polishing surface substantially adjacent to the perimeter portion of the wafer carrier while the wafer carrier moves the wafer over the polishing surface and wherein the body is movably attached to the wafer carrier.
4. The pad refurbisher of
5. The pad refurbisher of
6. The pad refurbisher of
7. The pad refurbisher of
8. The pad refurbisher of
9. The pad refurbisher of
10. The pad refurbisher of
11. The pad refurbisher of
12. The pad refurbisher of
16. The polishing machine of
17. The polishing machine of
18. The polishing machine of
19. The polishing machine of
20. The polishing machine of
21. The polishing machine of
22. The polishing machine of
23. The polishing machine of
24. The polishing machine of
26. The method of
27. The method of
28. The method of
29. The method of
30. The method of
0. 32. The pad refurbisher of
0. 33. The pad refurbisher of
0. 34. The pad refurbisher of
0. 35. The pad refurbisher of
0. 36. The pad refurbisher of
0. 37. The pad refurbisher of
0. 38. The pad refurbisher of
0. 39. The pad refurbisher of
0. 40. The pad refurbisher of
0. 42. The polishing machine of
0. 43. The polishing machine of
0. 44. The polishing machine of
0. 46. The method of
0. 47. The method of
0. 48. The method of
0. 49. The method of
0. 50. The method of
0. 51. The method of
0. 53. The pad refurbisher of
0. 54. The pad refurbisher of
0. 55. The pad refurbisher of
0. 56. The pad refurbisher of
0. 57. The pad refurbisher of
0. 58. The pad refurbisher of
0. 59. The pad refurbisher of
0. 60. The pad refurbisher of
0. 62. The polishing machine of
0. 63. The polishing machine of
0. 64. The polishing machine of
0. 66. The method of
0. 67. The method of
0. 68. The method of
0. 69. The method of
0. 70. The method of
0. 71. The method of
|
The present invention relates to an apparatus for selectively cleaning and conditioning the surface of a polishing pad used in chemical-mechanical polishing of semiconductor wafers and other microelectronic substrates.
Chemical-mechanical polishing (“CMP”) processes remove material from the surface of a wafer in the production of ultra-high density integrated circuits. In a typical CMP process, a wafer is pressed against a polishing pad in the presence of a slurry under controlled chemical, pressure, velocity, and temperature conditions. The slurry solution generally contains small, abrasive particles that abrade the surface of the wafer, and chemicals that etch and/or oxidize the surface of the wafer. The polishing pad is generally a planar pad made from a relatively soft, porous material such as blown polyurethane. Thus, when the pad and/or the wafer moves with respect to the other, material is removed from the surface of the wafer by the abrasive particles (mechanical removal) and by the chemicals in the slurry (chemical removal).
In the operation of the conventional planarizer 10, the wafer 12 is positioned face-downward against the polishing pad 40, and then the platen 20 and the wafer carrier 30 move relative to one another. As the face of the wafer 12 moves across the planarizing surface 42 of the polishing pad 40, the polishing pad 40 and the slurry 44 remove material from the wafer 12.
In the competitive semiconductor industry, it is desirable to maximize the throughput of the finished wafers and minimize the number of defective or impaired devices on each wafer. The throughput of CMP processes is a function of several factors, one of which is the rate at which the thickness of the wafer decreases as it is being planarized (the “polishing rate”). Because the polishing period per wafer decreases with increasing polishing rates, it is desirable to maximize the polishing rate within controlled limits to increase the number of finished wafers that are produced in a given period of time.
One problem with CMP processing is that the throughput may drop because the condition of the polishing surface on the pad deteriorates while polishing a wafer. The deterioration of the polishing pad surface is caused by waste particles from the wafer, pad, and slurry that accumulate on the polishing surface of the polishing pad. Since the accumulations of waste particles alter the condition of the polishing surface on the polishing pad, the polishing rate tends to drift over time. For example, after polishing a single wafer for only 4 minutes with a Rodel IC-1000 polishing pad and a Rodel ILD-1300 slurry (both of which are manufactured by Rodel Corp. of Arizona), the polishing rate drops and reduces the throughput for semiconductor wafers. Many semiconductor manufacturers accordingly recondition the pad after each wafer, but unless the reconditioning process is performed in situ and in real-time, then the reconditioning of the pad also causes down-time that reduces throughput. Thus, the waste particles on the polishing surface reduce the throughput of the CMP process.
CMP processes must also consistently and accurately produce a uniform, planar surface on the wafer because it is important to accurately focus the image of circuit patterns on the surface of the wafer. As the density of integrated circuits increases, it is often necessary to accurately focus the critical dimensions of the circuit pattern to better than a tolerance of approximately 0.1 μm. Focusing the circuit patterns to such small tolerances, however, is very difficult when the distance between the emission source and the surface of the wafer varies because the surface of the wafer is not uniformly planar. In fact, several devices may be defective on a wafer with a non-uniformnly uniformly planar surface. Thus, CMP processes must create a highly uniform, planar surface.
Another problem with CMP processing is that the accumulations of waste particles reduce the uniformity of the polished surface because they do not accumulate uniformly across the polishing surface of the pad. The polishing rate accordingly varies from one region on the pad to another resulting in a nonuniform polished surface on the wafer. Therefore, in light of the problems associated with accumulations of waste particles on polishing pads, it is necessary to periodically clean and condition the polishing surface to remove such accumulations and bring the polishing pad back to a desired condition.
Polishing surfaces on polishing pads are typically cleaned by brushing the pad with a brush, or by flushing the pad with a fluid. To perform the brushing and flushing processes, the wafer is generally removed from the pad while the brush or fluid engages the polishing surface of the polishing pad. One problem with the brushing and flushing processes, therefore, is that a significant amount of down-time is necessary to merely clean the polishing pad. Thus, it would be desirable to develop a pad cleaner that effectively cleans the pad in situ and in real-time.
Polishing surfaces of polishing pads are typically conditioned with a diamond embedded plate mounted to a separate device that moves the plate across the polishing pad to abrade the surface of the pad. Some pad conditioners remove a portion of the upper layer of the deteriorated polishing surface to form a new, clean polishing surface. One problem with conventional pad conditioners is that they condition the pad substantially uniformly across the polishing surface. Since the wafers only polish on a well-defined area of the pad (usually a concentric band spaced radially away from both the center of the pad and the perimeter of the pad), the pad conditioning needs to be performed proportionate to the pad surface wear. Moreover, it is desirable to condition a pad in situ and in real-time to avoid costly down-time associated with conditioning processes that stop the polishing of the wafer. Thus, it would be desirable to develop a device for selectively conditioning areas on the pad that require conditioning in situ and in real-time.
The inventive pad refurbisher provides in situ, real-time conditioning and/or cleaning of a polishing surface on a polishing pad used in chemical-mechanical polishing of a semiconductor wafer. The pad refurbisher has a body adapted for attachment to a wafer carrier of a chemical-mechanical polishing machine, and a refurbishing element connected to the body. The body has a face positioned proximate to a perimeter portion of the wafer carrier and facing generally toward the polishing surface of the polishing pad. The body travels with the wafer carrier as the wafer carrier moves over the polishing pad. The refurbishing element is connected to the face of the body so that the refurbishing element can operatively engage the polishing surface substantially adjacent to the perimeter of the wafer carrier. The refurbishing element is a pad conditioning device and/or a pad cleaning device that conditions and/or cleans the polishing surface of the pad to remove waste particles from the polishing surface of the polishing pad and place the pad in a desired polishing condition. In operation, the refurbishing element travels with the wafer carrier and is selectively engaged with the polishing surface while the wafer carrier presses the wafer against the polishing surface to selectively condition and/or clean generally only the deteriorated areas on the pad.
In one embodiment, the face of the body is a distal face defining a ring positioned radially outwardly from the perimeter of the wafer carrier, and the refurbishing element is either a diamond embedded pad conditioner or a brush-like pad cleaner. In another embodiment, the body has a first ring with a first refurbishing element and a second ring with a second refurbishing element. The first ring is positioned radially outwardly from the perimeter of the wafer carrier, and the second ring is positioned radially outwardly from the first ring. The first refurbishing element is preferably a brush-like pad cleaner and the second refurbishing element is preferably a diamond embedded pad conditioner.
The present invention is a CMP polishing pad refurbisher that selectively conditions and cleans generally only the deteriorated regions of a polishing surface on a polishing pad in situ and in real-time while a microelectronic substrate (e.g., a semiconductor wafer) is polished. An important aspect of the invention is that the pad refurbisher travels with the wafer carrier and positions a refurbishing element proximate to the wafer carrier without limiting the travel of the wafer carrier or over-conditioning unused regions on the polishing surface of the polishing pad. Another important aspect of the invention is that the refurbishing element may have a pad conditioner and a pad cleaner to simultaneously condition and clean the polishing surface in situ and in real-time while a wafer is polished. The pad refurbisher of the invention accordingly provides a clean and properly conditioned polishing surface on the polishing pad that enhances the uniformity of the finished surface on the wafer and the throughput of the CMP process.
The body 60 may be fixed to the wafer carrier 30, or as shown in
In a preferred embodiment, the body 60 is moved along the vertical axis Z—Z with respect to the wafer carrier 30 by a number of linear displacement actuators 80 positioned between a support member 63 attached to the body 60 and the top surface of the wafer carrier 30. The actuators 80 may be pneumatic cylinders, hydraulic cylinders, servomotors, springs, or any other suitable device that provides linear displacement between objects. The support member 63 may be a beam or plate connected to the body 60 (as shown in FIG. 2), or the support member may be made integrally with the body 60. A hole 65 through the support member 63 is positioned to slidably receive the shaft/actuator 36 of the wafer carrier 30 and allow the support member 63 to move along the vertical axis Z—Z with respect to the actuator 36. The actuators 80 preferably have a housing 82 attached to the wafer carrier 30 and an extensible rod 84 attached to the support member 63. As the rods 84 push against or pull on the support member 63, the body 60 moves upward or downward, respectively, along the vertical axis Z—Z with respect to the wafer carrier 30 to adjust the position of the distal face 62 with respect to the pad 40.
In other embodiments, the actuators 80 may act directly against the body 60 instead of the support member 63. For example, the actuator may be a motor (not shown) that rotates a drive gear (not shown) against a rack of teeth (not shown). The motor is connected to one of the wafer carrier 30 or the body 60, and the rack of teeth is positioned on the other of the wafer carrier 30 or the body 60. As the motor rotates the drive gear against the teeth, the drive gear moves the body 60 vertically with respect to the wafer carrier 30. Importantly, the actuator acts against the wafer carrier 30 and either the body 60 or a support member 63 connected to the body 60 to selectively move the body 60 vertically with respect to the wafer carrier 30 along the vertical axis Z—Z.
The actuators may be controlled manually or by a processor to selectively engage the refurbishing element 70 with the polishing surface 42 of the pad 40. In general, the refurbishing element 70 is selectively engaged with the polishing pad 40 on the areas of the planarizing surface 42 that contact the wafer 12. Since the wafer 12 usually contacts the pad 40 in a concentric band at a medial radial distance from the center of the pad 40, the actuators 80 are preferably controlled to lower the refurbishing element against the polishing surface 42 in the area defined by the concentric band. The actuators 80 may also control the pressure between the refurbishing element 70 and the pad 40 to provide a substantially constant pressure therebetween that does not affect the pressure between the wafer 12 and the pad 40. In one embodiment, the actuators 80 are manually set to position the body 60 so that the refurbishing element 70 engages the polishing surface 42 when the wafer carrier 30 presses the wafer 12 against the pad 40. To manually set the actuators, the wafer 12 is placed against a reference surface and then the refurbishing element 70 is lowered against the reference surface. The reference surface can be either the polishing pad 40 or another platform (not shown). In another embodiment, the actuators 80 are springs that bias the refurbishing element 70 against the polishing surface 42 to provide a substantially constant pressure between the refurbishing element 70 and the polishing pad 40. When the actuators are springs, the refurbishing element 70 is preferably positioned slightly below the face of the wafer 12 when the wafer 12 is off of the pad 40 so that the refurbishing element 70 engages the polishing surface 42 as the wafer carrier 30 presses the wafer 12 against the polishing pad 40.
In operation, the wafer carrier 30 is lowered to engage the wafer 12 with the polishing surface 42 of the polishing pad 40. As discussed above with respect to
The body 60 and the distal face 62 of the body 60 are shaped to position the refurbishing element 70 proximate to the perimeter of the wafer carrier 30 about at least a portion of the perimeter of the wafer carrier 30. For example, the body 60 may be attached to only a single side of the wafer carrier 30, and the body 60 may be shaped so that the distal face 62 and refurbishing element 70 are positioned asymmetrically about a fraction of the perimeter of the wafer carrier 30. In some instances, however, an asymmetrical mounting of the body 60 may impart asymmetrical forces on the wafer carrier 30. In particular, as the wafer carrier 30 rotates an asymmetrically positioned distal face 62 and refurbishing element 70 across the polishing pad 40, the centrifugal force of the refurbishing element 70 may cause the wafer carrier 30 to wobble. Also, since the polishing pad 40 will exert a force on the refurbishing element 70, an asymmetrically positioned refurbishing element 70 will cause the force between the wafer 12 and the polishing pad 40 to be uneven across the surface of the wafer 12. Accordingly, the body 60 is preferably shaped and attached to the wafer carrier 30 to symmetrically position the distal face 62 and refurbishing element 70 with respect to the center of the wafer carrier 30, thus reducing or eliminating any uneven forces on the wafer caused by an asymmetrical design.
In another embodiment, the inner and outer rings 61(a) and 61(b), respectively, of pad refurbisher 150 illustrated in
One advantage of the pad refurbishers 50 and 150 of the present invention is that they selectively condition and/or clean generally only the deteriorated areas on the polishing surface that need to be brought back to an acceptable polishing condition. By attaching the pad refurbisher to the wafer carrier so that the refurbishing element travels with the wafer carrier, and by controlling the vertical motion of the refurbishing element with respect to the wafer carrier, the refurbishing element may be selectively engaged with the deteriorated areas on the pad. Moreover, by positioning the refurbishing element proximate to the wafer carrier, only a slightly larger area than that of the wafer carrier is conditioned or cleaned even when the refurbishing element continuously engages the pad. Therefore, compared to conventional conditioners, the pad refurbisher of the present invention reduces over-conditioning of areas on the polishing surface that do not require conditioning or cleaning.
Another advantage of the present invention is that the pad refurbishers 50 and 150 condition and/or clean a polishing surface of a polishing pad in situ and in real-time while a wafer is planarized. Since the cleansing element 70 may be selectively engaged and disengaged with the polishing pad from the wafer carrier 30, the wafer 12 may be polished while the polishing surface 42 of the pad 40 is conditioned and/or cleaned. Thus, compared to some conditioning devices that cannot simultaneously condition the pad and polish the wafer, the pad refurbisher 50 enhances the throughput of the CMP process because the down-time to condition and clean the polishing pad is significantly reduced or even eliminated.
From the foregoing it will be appreciated that, although specific embodiments of the invention have been described herein for purposes of illustration, various modifications may be made without deviating from the spirit and scope of the invention. For example, the apparatus and method may also be used in chemical-mechanical polishing of other microelectronic substrates, such as field emission displays, in addition to semiconductor wafers. Accordingly, the invention is not limited except as by the appended claims.
Sandhu, Gurtej S., Doan, Trung T.
Patent | Priority | Assignee | Title |
10265829, | Oct 30 2015 | TAIWAN SEMICONDUCTOR MANUFACTURING CO , LTD | Chemical mechanical polishing system |
10300578, | Dec 13 2013 | Taiwan Semiconductor Manufacturing Co., Ltd. | Carrier head having abrasive structure on retainer ring |
7909910, | Oct 07 2006 | TBW Industries Inc. | Vacuum line clean-out separator system |
9120195, | Feb 20 2009 | ALUDYNE NORTH AMERICA, INC | Wheel assembly and method for making same |
9604340, | Dec 13 2013 | Taiwan Semiconductor Manufacturing Co., Ltd. | Carrier head having abrasive structure on retainer ring |
9782871, | Jan 29 2009 | Lawrence Livermore National Security, LLC | Apparatus and method for deterministic control of surface figure during full aperture pad polishing |
Patent | Priority | Assignee | Title |
5584751, | Feb 28 1995 | Ebara Corporation | Wafer polishing apparatus |
5595527, | Jul 27 1994 | Texas Instruments Incorporated | Application of semiconductor IC fabrication techniques to the manufacturing of a conditioning head for pad conditioning during chemical-mechanical polish |
5664987, | Jan 31 1994 | National Semiconductor Corporation | Methods and apparatus for control of polishing pad conditioning for wafer planarization |
5749771, | Feb 22 1994 | NEC Electronics Corporation | Polishing apparatus for finishing semiconductor wafer at high polishing rate under economical running cost |
5775983, | May 01 1995 | Applied Materials, Inc.; Applied Materials, Inc | Apparatus and method for conditioning a chemical mechanical polishing pad |
5782675, | Oct 21 1996 | U S BANK NATIONAL ASSOCIATION, AS COLLATERAL AGENT | Apparatus and method for refurbishing fixed-abrasive polishing pads used in chemical-mechanical planarization of semiconductor wafers |
5785585, | Sep 18 1995 | GLOBALFOUNDRIES Inc | Polish pad conditioner with radial compensation |
5823854, | May 28 1996 | TRANSPACIFIC IP LTD , | Chemical-mechanical polish (CMP) pad conditioner |
5851138, | Aug 05 1997 | Texas Instruments Incorporated | Polishing pad conditioning system and method |
5857899, | Apr 04 1997 | Applied Materials, Inc | Wafer polishing head with pad dressing element |
5885137, | Jun 27 1997 | Polaris Innovations Limited | Chemical mechanical polishing pad conditioner |
5885147, | May 12 1997 | Novellus Systems, Inc | Apparatus for conditioning polishing pads |
5902173, | Mar 19 1996 | Yamaha Corporation | Polishing machine with efficient polishing and dressing |
5931725, | Jul 30 1996 | Tokyo Seimitsu Co., Ltd. | Wafer polishing machine |
6004193, | Jul 17 1997 | Bell Semiconductor, LLC | Dual purpose retaining ring and polishing pad conditioner |
6019670, | Mar 10 1997 | Applied Materials, Inc. | Method and apparatus for conditioning a polishing pad in a chemical mechanical polishing system |
6077155, | Apr 14 1995 | Sony Corporation | Polishing device and correcting method therefor |
6135868, | Feb 11 1998 | Applied Materials, Inc | Groove cleaning device for chemical-mechanical polishing |
Executed on | Assignor | Assignee | Conveyance | Frame | Reel | Doc |
Dec 19 2001 | Micron Technology, Inc. | (assignment on the face of the patent) | / | |||
Apr 26 2016 | Micron Technology, Inc | U S BANK NATIONAL ASSOCIATION, AS COLLATERAL AGENT | SECURITY INTEREST SEE DOCUMENT FOR DETAILS | 038669 | /0001 | |
Apr 26 2016 | Micron Technology, Inc | MORGAN STANLEY SENIOR FUNDING, INC , AS COLLATERAL AGENT | PATENT SECURITY AGREEMENT | 038954 | /0001 | |
Apr 26 2016 | Micron Technology, Inc | U S BANK NATIONAL ASSOCIATION, AS COLLATERAL AGENT | CORRECTIVE ASSIGNMENT TO CORRECT THE REPLACE ERRONEOUSLY FILED PATENT #7358718 WITH THE CORRECT PATENT #7358178 PREVIOUSLY RECORDED ON REEL 038669 FRAME 0001 ASSIGNOR S HEREBY CONFIRMS THE SECURITY INTEREST | 043079 | /0001 | |
Jun 29 2018 | U S BANK NATIONAL ASSOCIATION, AS COLLATERAL AGENT | Micron Technology, Inc | RELEASE BY SECURED PARTY SEE DOCUMENT FOR DETAILS | 047243 | /0001 | |
Jul 31 2019 | MORGAN STANLEY SENIOR FUNDING, INC , AS COLLATERAL AGENT | Micron Technology, Inc | RELEASE BY SECURED PARTY SEE DOCUMENT FOR DETAILS | 050937 | /0001 |
Date | Maintenance Fee Events |
Sep 20 2005 | ASPN: Payor Number Assigned. |
May 25 2007 | M1552: Payment of Maintenance Fee, 8th Year, Large Entity. |
May 25 2011 | M1553: Payment of Maintenance Fee, 12th Year, Large Entity. |
Date | Maintenance Schedule |
Jul 18 2009 | 4 years fee payment window open |
Jan 18 2010 | 6 months grace period start (w surcharge) |
Jul 18 2010 | patent expiry (for year 4) |
Jul 18 2012 | 2 years to revive unintentionally abandoned end. (for year 4) |
Jul 18 2013 | 8 years fee payment window open |
Jan 18 2014 | 6 months grace period start (w surcharge) |
Jul 18 2014 | patent expiry (for year 8) |
Jul 18 2016 | 2 years to revive unintentionally abandoned end. (for year 8) |
Jul 18 2017 | 12 years fee payment window open |
Jan 18 2018 | 6 months grace period start (w surcharge) |
Jul 18 2018 | patent expiry (for year 12) |
Jul 18 2020 | 2 years to revive unintentionally abandoned end. (for year 12) |